Master Bond Test Results
Testing Lap Shear Strength of Adhesives for Bonding Polycarbonate
 
 
 
 
 
 
Master Bond technical experts test the lap shear strength of various epoxy compounds utilized for bonding polycarbonate to polycarbonate substrates. Testing was based on ASTM D1002, where two polycarbonate coupons were bonded together and then pulled apart in shear. Find out which compounds work best for polycarbonate bonding when considering other factors such as temperature range, chemical resistance requirements, processing considerations and more.
High Lap Shear Strength Adhesives for Bonding Polycarbonate
 
 
 
Master Bond Product EP21ARHT
EP21ARHT
High strength epoxy offers superior acid resistance
Request a Technical Datasheet
Master Bond Product EP21LV
EP21LV
Low viscosity epoxy meets FDA requirements
Request a Technical Datasheet
Master Bond Product EP30-2
EP30-2
High strength, low viscosity epoxy offers optical clarity
Request a Technical Datasheet
Master Bond Product EP29LPSP
EP29LPSP
Cryogenically serviceable, NASA low outgassing epoxy
Request a Technical Datasheet
Master Bond Product EP31ND
EP31ND
Smooth paste epoxy offers superior electrical insulation
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2023 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.