Having trouble viewing images? View email in browser
|
|
|
 |
|
| EP114: Utilized to produce nanocomposites via vacuum infiltration |
|
| Researchers at Florida International University used epoxy system EP114 for creating robust nanocomposites by vacuum infiltrating graphene and boron nitride nanoplatelet foams. The epoxy ensured even dispersion of nanoparticles, enhancing the structural integrity and thermal resilience of the composites while preventing particle aggregation. |
|
|
|
|
|
|
|
|
|
|
|
| Two Part, Optically Clear Epoxy EP114 |
|
| This epoxy features a low viscosity and very long open time with an exceptionally low shrinkage upon curing and excellent dimensional stability. |
|
|
|
|
|
|
|
|
|
|
|
|
|
|