EP15: Utilized to test the bond strength of thermal spray coatings according to ASTM C633
Epoxy system EP15 features a high tensile strength in excess of 12,000 psi, making it ideal for testing adhesive and cohesive strengths of various thermal spray coatings according to ASTM C633 standards. Read through to learn more about this unique testing process along with 6 case studies which provide an overview of the uses of EP15 in real-world applications.
Master Bond Product EP15
One Part Epoxy System EP15
Master Bond EP15 is a heat curing epoxy featuring high tensile strength in excess of 12,000 psi that forms dimensionally stable bonds.
Request a Technical Datasheet
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2024 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.