| MasterSil 800: Used as a High-Temperature Encapsulant for a Wide-Bandgap Semiconductor |
|
| A wide-bandgap semiconductor device required a high-temperature encapsulant to ensure protection against environmental factors and thermal stress in extreme operating conditions. Master Bond's MasterSil 800, a two-component silicone elastomer, was chosen for this application due to its outstanding thermal stability, flexibility, and electrical insulation properties. |
|
|
|
|
|
|
|
|
|
|
|
| One Part Silicone Elastomer MasterSil 800 |
|
| MasterSil 800 is a high performance silicone elastomer designed for bonding, sealing, coating, and form in-place gaskets, featuring exceptional high-temperature resistance up to 572°F (300°C). |
|
|
|
|
|
|
|
|
|
|
|
|
|
|