UL Certified Arc Resistant Epoxy
logo
Electrical arcing occurs when a current from one electrical connection jumps to another, and upon exposure to its surrounding environment creates a flash of electricity. This can result in combustion or fire, and leads to the degradation of the surrounding material and components within the electrical device.
Electrical Device
Common causes of electrical arcing:
Bullet Breaks in the electrical insulation
Bullet Corrosion
Bullet Faulty insulation
bullet Exposed surfaces on the conductor
As a consequence, arc suppression is critical for the safety and reliability of manufactured electrical devices. Some epoxy compounds have been specifically formulated to resist electrical arcing – protecting the wiring and its surrounding components from ignition. These compounds do not ignite even after exposure to over 150 arcs during the UL 746A High Amp Arc Ignition test.
Epoxy System EP21AC
Arc Ignition Resistant Epoxy EP21AC
Ideal for encapsulating and coating applications, EP21AC passed UL 746A High Amp Arc Ignition test with the highest rating (Performance Level Category or PLC of 0). This epoxy compound, when cured at a thickness of 3.0 mm, withstood over 150 arcs without ignition. It also passed the UL 94HB flammability test.
Learn more
Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2024 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.