EP42HT-4AOMed Black
Medical Grade Epoxy Offers Thermal Conductivity and Electrical Insulation
Master Bond New Product Release

Master Bond EP42HT-4AOMed Black is a new two part epoxy created for medical device manufacturing. It is biocompatible and non-cytotoxic, passing both USP Class VI and ISO 10993-5 certifications. This epoxy withstands aggressive chemical sterilants, radiation and repeated cycles of autoclaving.

EP42HT-4AOMed Black offers both cryogenic serviceability and heat resistance with a service temperature range from 4K to 400°F. Its thermal conductivity measures 9-10 BTU•in/(ft2•hr•°F) and its volume resistivity is greater than 1014 ohm-cm. The system contains a filler, which contributes to its high strength profile and dimensional stability. This adhesive bonds well to metals, composites, glass, ceramics, rubbers and plastics and features a tensile modulus of 500,000-550,000 psi, a compressive strength of 24,000-26,000 psi, and a tensile strength of 7,000-8,000 psi.

This epoxy can cure at room temperature, yet faster cures can be achieved by heat curing. In order to obtain optimal properties, an overnight cure at room temperature, followed by heat curing at 150-200°F for 2-3 hours is recommended. The mix ratio is 100 to 40 by weight. Once mixed, this versatile adhesive has very good flow properties, making it suitable for bonding, sealing and coating applications. Upon curing, EP42HT-4AOMed Black exhibits very low shrinkage, low exotherm and can be used for castings up to 2-3 inches thick. This opaque black epoxy is available in the following size kits: ½ pint, pint, quart and gallon. It is also available in pre-mixed and frozen syringes, which are compatible with automated dispensing equipment.

Master Bond Facebook Master Bond LinkedIn Master Bond Twitter Master Bond LinkedIn

Master Bond Inc. | www.masterbond.com | [email protected] | +1.201.343.8983
154 Hobart Street, Hackensack, New Jersey 07601 USA


Copyright © 2019 by Master Bond Inc. All Rights Reserved.
This content may not be reproduced in any way without the prior written permission of Master Bond Inc.