Key Features
• Nanosilica filled system
• Serviceability from
-60°F to +300°F
• Superior optical clarity
• Excellent hardness and abrasion resistance |
Electrical Properties
• Volume resistivity of 1.5x109 megohm-cm
• Dielectric constant of 3.16 at 75°F
• Dissipation factor of 0.005 at 75°F
|
Cure Schedule
• 5-10 sec. using light emitting 250-365 nm wavelength & 20-40 milliwatts/cm2 energy output
• Post cure of 200-
230°F for 30 min. enhances temperature resistance
|
Industries
• Electro-optic
• Fiber-optic
• Electronic
• Optical
|