Non-Drip Adhesive Systems
|
Unlike the Autumn Leaves,
Our Non-Drip Epoxy Won't Fall
Master Bond Supreme 10HTND-3
blends high shear and peel strengths in excess of 3,600 psi and up to
30 pli, respectively, with a totally non-drip application feature. This
one component epoxy has a number of outstanding processing advantages
including an unlimited working life at room temperature, no mixing prior
to use, a viscosity that remains constant and will not thicken with
time and it is room temperature storable.
It is a toughened
system that readily withstands severe thermal cycling along with
mechanical shock and vibration. Supreme 10HTND-3 is cryogenically
serviceable and has an exceptionally wide temperature range of 4K to
+400°F. Some additional advantages include:
-
High bond strength to similar and dissimilar substrates
-
Superior electrical insulation properties
-
Excellent resistance to many chemicals including water, oils, fuels, solvents acids and bases
-
100% reactive; contains no solvents or diluents
-
Versatile cure schedules: 60-75 minutes at 250°F; 35-45 minutes at 300°F
|