EP41S-1HT
Two Component, Room Temperature Curing Epoxy Compound
|
Spotlight-2
Key Features
 
Withstands high temperatures

• Serviceability from -60°F to +400°F

• Exceptional bond strength

• Good electrical insulation properties
Chemical Resistance
 
Superior ability to resist prolonged immersion to:

• Solvents
• Fuels
• Oils
• Alcohols

• Acids
• Water
 
Cure Schedules
 
24-48 hours at 75°F

• 1-2 hours
at 200°F


To optimize chemical resistance properties, it is recommended to add heat.

 
Industries
 
• Chemical processing

• Automotive

 
Master Bond EP41S-1HT is a two component epoxy system with outstanding resistance to a variety of chemicals including gasoline, gasohol, fuels, oils, alcohols, methyl, ethyl, butyl, ethyl acetates, toluene, as well as a wide number of other organic and inorganic solvents. In addition to its ability to withstand chemical immersions, this low viscosity system has excellent mechanical properties including high tensile and compressive strengths.

EP41S-1HT is 100% reactive and contains no solvents or diluents. Its linear shrinkage upon cure is very low—less than 0.1% inches/inch. It is serviceable over the wide temperature range of -60°F to +400°F. This system adheres well to a wide variety of substrates including metals, glass, ceramics, rubbers and many plastics.

For more detailed information on EP41S-1HT, please visit our product description.
Master Bond | 154 Hobart Street | Hackensack, NJ 07601 | Phone: +1 201-343-8983 | Fax: +1 201-343-2132  [email protected] | www.masterbond.com