Master Bond Inc.
Having trouble viewing images? View email in browser
Nanosilica Filled Epoxy Features Unmatched Abrasion Resistance Properties
 
 
 
 
Offers excellent physical strength profile and resists exposure to harsh wear and scraping
Master Bond Video
Independent tests demonstrate that this epoxy’s abrasion resistance value is significantly higher than that of a typical epoxy composition. EP30NS is also optically clear and meets NASA low outgassing specifications. Watch now to learn more about EP30NS.