Is there an adhesive that is chemically resistant to acetone?

This application  discusses adhesive systems that provide excellent resistance to acetone and other harsh chemicals in demanding industrial environments. It also reviews key selection factors such as chemical compatibility, operating temperature, substrate adhesion and long-term durability to help ensure reliable performance.

Imagen
EP41S-1 Master Bond Epoxy

The Application

Customer wants to build a special wafer carrier that has aluminum parts glued together. The carrier is eventually to be soaked in acetone.

Finding the Answers

  • What temperature does the exposure to acetone take place?
  • What is the duration of exposure and how many times does this exposure occur?
  • Do you want low outgassing?
  • What viscosity are you looking for?

The Solution

Master Bond offers a variety of compounds that resist harsh chemicals

Making certain assumptions about the answers to the above questions, Venkat recommended EP41S-1.

EP41S-1 has outstanding chemical resistance. It was tested as a coating of about 0.020 inches thick on sand blasted steel. To optimize its chemical resistance, it was cured for 24 hours at room temperature followed by 2-3 hours at 200°F. The system was then immersed in a wide variety of chemicals including ethylene glycol, sodium hydroxide, toluene, gasoline, and more, for over 1 year. After 14 months, no failures were observed.

The operating temperature of EP41S-1 ranges from -60°F to +300°F. The viscosity of Part A is 10,000-15,000 and Part B is 250-400.

EP41S-1 also comes in a non-drip version, EP41S-1ND, and in a high temperature version, EP41S-1HT which is serviceable up to 400°F.

Summary of Products

ProductChemistryViscosityService Temperature Range
EP41S-1Two part epoxyLow-60°F to +300°F
EP41S-1NDTwo part epoxyNon-drip-60°F to +300°F
EP41S-1HTTwo part epoxyModerate-60°F to +400°F
EP62-1Two part epoxyLow-60°F to +450°F
EP21ARHTTwo part epoxyModerate-60°F to +400°F
EP21ARHTNDTwo part epoxyNon-drip-60°F to +400°F
EP42HT-2Two part epoxyLow-60°F to +450°F

Meet Our Tech Expert: Venkat Nandivada

imageVenkat Nandivada has been the Manager of Technical Sales at Master Bond Inc since 2010. He has a Masters degree in Chemical Engineering from Carnegie Mellon University. His hobbies include table tennis, cricket and soccer.