Supreme 3HTND-2DM-1
One component epoxy featuring non drip consistency for bonding, sealing and specialty dam-and-fill encapsulation
Key Features
- Toughened system
- Fast curing
- Good physical strength properties
- Convenient packaging and dispensing
Typical Properties
Viscosity
paste
Cure Schedule
20-30 minutes at 250°F or 5-10 minutes at 300°F
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +400°F
Dielectric Constant
4.6 @ 75°F, 60 Hz
Tensile Modulus
300,000-350,000 psi