EP38FLAO is no longer available. We recommend EP37-3FLFAO as a potential alternative. Please consult with our technical team to verify that this replacement is the most appropriate solution for your application.
Recommended Replacement Product
Imagen
Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting.