One Part Epoxy EP15
EP15
One part epoxy for testing adhesion or cohesive strength of ceramic based flame-sprayed coatings
Tensile Strength
12,000-14,000 psi
Tensile Lap Shear Strength
2,600-2,800 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
40,000-65,000 cps 300-350°F for 60-90 minutes, with an optimum cure schedule of 60-90 minutes at 300-350°F plus post cure 4-6 hours at 300-350°F 80-90 Shore D -60°F to +250°F /es/tds/ep15
EP17HT-LO One Part Epoxy
EP17HT-LO
One component epoxy system for bonding, sealing, coating and casting
Glass Transition Temperature (Tg)
200-210°C
Tensile Lap Shear Strength
3,000-3,200 psi at 75°F
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
45,000-75,000 cps 300°F for 4-6 hours, plus 12-24 hours at 350°F 80-90 Shore D -80°F to +600°F /es/tds/ep17ht-lo
One Part Epoxy EP3HT-LO
EP3HT-LO
One part, heat curing, no mix epoxy system
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
100,000-200,000 cps 250°F for 20-30 minutes or 300°F for 5-10 minutes, followed by 1 to 3 hours at 250 to 300°F 80-90 Shore D -60°F to +400°F /es/tds/ep3ht-lo
One Part, Silver Filled Epoxy EP3HTS-TC
EP3HTS-TC
One component, silver filled epoxy featuring extraordinary electrical and thermal conductivity
Thermal Conductivity
110-118 BTU•in/(ft²•hr•°F) [16-17 W/(m•K)]
Volume Resistivity
<1x10⁻³ ohm-cm
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Die Attach
  • Sealing
  • Coating
paste Cures rapidly at 250 to 300°F 60-70 Shore D -80°F to +400°F /es/tds/ep3hts-tc
EP3HTSDA-2 One Part Die Attach Epoxy
EP3HTSDA-2
One component epoxy system featuring excellent electrical and thermal conductivity
Thermal Conductivity
45-49 BTU•in/(ft²•hr•°F) [6.5-7 W/(m•K)]
Volume Resistivity
<0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Die Attach
  • Gap Filling
  • Sealing
  • Coating
>400,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes, optimum cure schedule is either option above, plus 1 hour at 250-300°F 75-85 Shore D -80°F to +450°F /es/tds/ep3htsda-2
EP4EN-80 One Component Epoxy
EP4EN-80
One component flowable epoxy for bonding and small encapsulation applications with a curing schedule at 80°C to 85°C
Dielectric Constant
4.4
Thermal Conductivity
5.2-5.9 BTU•in/(ft²•hr•°F) [0.75-0.85 W/(m•K)]
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Encapsulation
  • Potting
600-1,800 cps 90 minutes at 65°C plus 30 minutes at 80-85°C 85-95 Shore D -58°F to +302°F /es/tds/ep4en-80
EP5G-80 One Component Epoxy
EP5G-80
One component, graphite filled epoxy with a curing temperature of 80°C
Glass Transition Temperature (Tg)
130-140°C
Volume Resistivity
5-15 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
30,000-300,000 cps 4 hours at 80°C 75-85 Shore D -58°F to +347°F /es/tds/ep5g-80
EP5TC-80 One Component Paste Epoxy
EP5TC-80
One component thermally conductive, electrically insulating epoxy with a curing temperature of 80°C
Dielectric Constant
4.6
Volume Resistivity
>10¹² ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
60,000-180,000 cps 80°C for 90-120 minutes with an optional post cure of 1-2 hours at 80°C to optimize properties 90-100 Shore D -58°F to +302°F /es/tds/ep5tc-80
Supreme 3HT-80 One Component Epoxy System
Supreme 3HT-80
One component, toughened epoxy adhesive, sealant and coating
Dielectric Constant
3.8
Tensile Lap Shear Strength
600-800 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
70,000-150,000 cps 175-180°F 45-50 minutes, 250°F 20-30 minutes 75-85 Shore D -100°F to +350°F /es/tds/supreme-3ht-80
EP101HTX-3 One Part Epoxy System
EP101HTX-3
One component epoxy system for impregnation, bonding, sealing and coating
Glass Transition Temperature (Tg)
170-175°C
Volume Resistivity
>3 x 10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
300-1,000 cps 6 to 8 hours at 300°F followed by 2 to 3 hours at 350°F 80-90 Shore D -60°F to +500°F /es/tds/ep101htx-3