EP101HTX-3
One component epoxy system for impregnation, bonding, sealing and coating
Key Features
- Very low viscosity
- Unlimited working life at room temperature
- High temperature resistant
- Superior electrical insulator
Typical Properties
Viscosity
300-1,000 cps
Cure Schedule
6 to 8 hours at 300°F followed by 2 to 3 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +500°F
Glass Transition Temperature (Tg)
170-175°C
Volume Resistivity
>3 x 10¹⁴ ohm-cm