UV10TK40RCL
Red colored UV curable epoxy acrylate system turns clear upon exposure to UV light
Dielectric Constant
3.9
Refractive Index
1.55
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
30,000-60,000 cps UV light 325-365 nm for 30-90 seconds after the color change 75-85 Shore D -60°F to +450°F /es/tds/uv10tk40rcl
UV10TKLO-2 One Component UV Curable Compound
UV10TKLO-2
One component UV-curable system for bonding, sealing and encapsulation
Dielectric Constant
3.6
Tensile Modulus
>200,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
225,000-275,000 cps UV light 320-365 nm for 20-30 seconds 80-85 Shore D -60°F to +400°F /es/tds/uv10tklo-2
UV15 One Part UV Curable Compound
UV15
Low viscosity, one component, UV curable epoxy based system
Glass Transition Temperature (Tg)
90-95°C with a straight UV cure; 125-130°C when post cured for 30 minutes at 125°C.
Refractive Index
1.517
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • IEC 61249-2-21 for Halogen Free
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
115-350 cps Cures in thicknesses of a few microns to 0.015-0.020 inches in 15-30 seconds or less. >75 Shore D -80°F to +350°F. /es/tds/uv15
UV15-42C One Part UV System
UV15-42C
One component UV system for high performance bonding, coating and sealing
Dielectric Constant
4.2
Elongation
10-20%
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2 >60 Shore D -65°F to +300°F /es/tds/uv15-42c
UV15-7DCNV-1 One Part UV Adhesive
UV15-7DCNV-1

One part, dual cure UV system for high performance bonding, sealing, coating and encapsulation
 

Refractive Index
1.54
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Cures in 15-45 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm² 70-80 Shore D -80°F to +300°F /es/tds/uv15-7dcnv-1
UV15-7HP
One part UV system for high performance bonding, sealing, coating and encapsulation
Refractive Index
1.54
Tensile Modulus
250,000-350,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
300-1,500 cps Cures in 15-45 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2. 70-80 Shore D -80°F to +300°F /es/tds/uv15-7hp
UV15-7LRI One Part UV System
UV15-7LRI
One part, UV curable polymer system for bonding, sealing, coating and encapsulating
Refractive Index
1.481
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
2,000-4,000 cps cures quickly in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm² 55-65 Shore D -60°F to +250°F /es/tds/uv15-7lri
UV15-7NS
One part nanosilica filled UV curable system
Coefficient of Thermal Expansion
30-35 X 10⁻⁶ in/in/°C
Refractive Index
1.55
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
100-700 cps UV15-7NS will cure quickly and easily at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². UV15-7NS normally cures in 20-30 seconds under appropriate conditions. 85-95 Shore D -80°F to +300°F /es/tds/uv15-7ns
UV15-7TK1ANV-3 One Part UV Curable Adhesive
UV15-7TK1ANV-3
One component, paste consistency UV curable system
Dielectric Constant
3.4
Tensile Modulus
300,000-350,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Coating
paste 15-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output of 20 milliwatts/cm2 70-80 Shore D -80°F to +300°F /es/tds/uv15-7tk1anv-3
UV15DC80-1
One component, UV and heat curable epoxy compound with moderate viscosity
Glass Transition Temperature (Tg)
125-135°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Coating
  • Sealing
  • Encapsulation
  • Gap Filling
20,000-40,000 cps 10-20 seconds with UV light at 365 nm with 20-40 milliwatts/cm2 of energy; 80°C for 60-90 minutes; post curing for 2-4 hours; 1-2 hours at 125°C >70 Shore D -80°F to +350°F /es/tds/uv15dc80-1