UV15DC80-1
One component, UV and heat curable epoxy compound with moderate viscosity
Key Features
- Allows for curing in “shadowed out” areas
- Cures at temperatures as low as 80°C
- Excellent physical strength properties
- NASA low outgassing
Typical Properties
Viscosity
20,000-40,000 cps
Cure Schedule
10-20 seconds with UV light at 365 nm with 20-40 milliwatts/cm2 of energy; 80°C for 60-90 minutes; post curing for 2-4 hours; 1-2 hours at 125°C
Hardness
>70 Shore D
Service Temperature Range
-80°F to +350°F
Glass Transition Temperature (Tg)
125-135°C
Volume Resistivity
>10¹⁴ ohm-cm
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863