Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP110F8-5 Two Part Epoxy
EP110F8-5
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Coefficient of Thermal Expansion
60-70 in/in X 10⁻⁶/°C
Tensile Modulus
35,000-65,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Potting
  • Sealing
  • Encapsulation
  • Coating
  • Bonding
  • Gap Filling
7,000-11,000 cps 4-6 hours at 250-300°F 70-80 Shore D -100°F to +300°F /es/tds/ep110f8-5
EP112 Two Part Epoxy
EP112
Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation
Refractive Index
1.55
Volume Resistivity
>10¹⁴ ohm-cm
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Impregnation
  • Gap Filling
50-200 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F 75-90 Shore D -60°F to +450°F /es/tds/ep112
EP121CL-LO Two Part Epoxy
EP121CL-LO
Two component epoxy for potting, encapsulation, coating and sealing applications
Dielectric Constant
3.25
Refractive Index
1.56
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Potting
  • Encapsulation
  • Sealing
  • Coating
  • Bonding
1,000-3,000 cps 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F 80-90 Shore D -80°F to +500°F /es/tds/ep121cl-lo
Epoxy System EP125
EP125
Two part epoxy for bonding and sealing featuring very high temperature resistance
Dielectric Constant
3.9
Tensile Lap Shear Strength
2,500-2,700 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250,000-500,000 cps 3-4 hours at 300°F or 2-3 hours at 350°F 85-95 Shore D -80°F to +600°F /es/tds/ep125
EP126 Two Component Epoxy Compound
EP126
Two part epoxy for bonding and sealing featuring very high temperature resistance
Dissipation Factor
0.091 @ 75F; 0.034 @ 500F
Glass Transition Temperature (Tg)
160 to 180°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250,000-500,000 cps 3-4 hours at 300°F or 2-3 hours at 350°F -80°F to +600°F /es/tds/ep126
Two Part Epoxy EP126TK
EP126TK
Two part non-drip epoxy for bonding and sealing featuring very high temperature resistance
Dielectric Constant
3.9
Glass Transition Temperature (Tg)
160 to 180°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 3-4 hours at 300°F or 2-3 hours at 350°F; post curing for 12-24 hours at 400-450°F -80°F to +600°F /es/tds/ep126tk
EP13 One Part Epoxy System
EP13
One component, heat curing epoxy for structural bonding applications
Dielectric Constant
4.5
Tensile Lap Shear Strength
3,500 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 60-90 minutes at 300-350°F 80-85 Shore D -60°F to +500°F /es/tds/ep13
EP13LTE One Part Epoxy
EP13LTE
One component, heat curing epoxy for structural bonding applications featuring low coefficient of thermal expansion
Coefficient of Thermal Expansion
15-20 X 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
155-160°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
paste 300-350°F for 1-2 hours; post cure of 2-3 hours at 350-400°F 85-95 Shore D -60°F to +500°F /es/tds/ep13lte
EP13SPND-2 One Part Heat Cure Epoxy
EP13SPND-2
One component, heat curing epoxy for structural bonding applications
Dielectric Constant
4.9
Tensile Lap Shear Strength
3,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Gap Filling
paste 300-350°F for 60-90 minutes, post cure at 350-400°F for 2 hours 85-90 Shore D -60°F to +500°F /tds/ep13spnd-2
One Part Epoxy EP15ND-2
EP15ND-2
One part epoxy for testing adhesion or cohesive strength of metallic based flame-sprayed coatings
Tensile Strength
12,000-14,000 psi
Tensile Lap Shear Strength
2,600-2,800 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
paste 300-350°F for 60-90 minutes 80-90 Shore D -60°F to +250°F /es/tds/ep15nd-2

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).