EP21FRNS-2
Two component epoxy system for potting, encapsulating and casting
Key Features
- Meets UL 94V-0 flame retardant specification
- Features a non-halogen filler
- Produces very low smoke levels
- Cures at room temperature
Typical Properties
Viscosity
Part A: 40,000-70,000 cps, Part B: 30,000-45,000 cps
Cure Schedule
Cures at 75°F, 48-72 hours
Hardness
>75 Shore D
Service Temperature Range
-59.8°F to +194°F
Dielectric Constant
4.5
Tensile Lap Shear Strength
>1,200 psi
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
UL 94V-0 Flame Resistant