EP30LP-2
High performance two part epoxy for bonding, coating, sealing and encapsulation
Key Features
- Very low viscosity
- Superb optical clarity and light transmission properties
- Exceptionally low shrinkage
- Passes NASA low outgassing requirements
Typical Properties
Viscosity
Part A: 900-1,600 cps, Part B: 100-400 cps
Cure Schedule
overnight at 75°F, followed by 2-3 hours at 150°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Strength
440 volts/mil
Refractive Index
1.56