EP30NG
Two component, room temperature curing epoxy containing graphene filler
Key Features
- Exceptionally high thermal conductivity
- High compressive strength
- Superior dimensional stability
- Low thermal expansion coefficient
Typical Properties
Viscosity
paste
Cure Schedule
At 75°F, the Master Bond Polymer System EP3ONG cures in 4-5 days. Faster cures can be realized at elevated temperatures, e.g., 3-5 hours at 150-200°F. The optimal cure schedule is overnight at 75°F followed by 4-6 hours at 150-200°F.
Hardness
85-95 Shore D
Service Temperature Range
-60°F to +300°F
Thermal Conductivity
38.15 BTU•in/(ft²•hr•°F) [5.5 W/(m•K)]
Volume Resistivity
100-200 ohm-cm