EP35SP
Two component epoxy system for bonding, sealing and coating applications
Key Features
- Exceptionally high glass transition temperature
- Very long open time
- Paste consistency
- Resists aggressive chemicals
Typical Properties
Viscosity
paste
Cure Schedule
1 hour at 110°C, followed by 2 to 3 hours at 125-150°C, with a post cure at 175°C for 2 to 3 hours
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +550°F
Glass Transition Temperature (Tg)
215-220°C
Tensile Lap Shear Strength
2,200-2,400 psi