EP3FL

One component epoxy system for bonding, sealing and coating
Key Features
  • No mixing and convenient processing
  • Toughened system
  • Wide service temperature range of -100°F to +300°F
  • Superb thermal and electrical insulator
Typical Properties
Viscosity
60,000-90,000 cps
Cure Schedule
250°F for 20-30 minutes; 300°F for 5-10 minutes
Hardness
75-85 Shore D
Service Temperature Range
-100°F to +300°F
Dielectric Constant
3.7
Volume Resistivity
>10¹⁴ ohm-cm
Imagen
EP3FL One Part Epoxy Compound
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP3FL is a one part system that offers easy processing along with excellent physical strength and adhesive properties. It is a true one part system, not premixed and frozen, and can be stored either at room temperature or in a refrigerator. The system does, however, require oven curing with a minimum temperature of 250°F. As noted in the table, it cures rapidly at 250°F and even more quickly at 300°F. In essence, it has an unlimited working life at room temperature. Also, it is a toughened or slightly flexibilized system. This allows the system to withstand rigorous thermal cycling and shock.

EP3FL bonds well to a wide variety of substrates including glass, metals, composites, ceramics and many plastics. It has good chemical resistance to water, oils, fuels and hydraulic fluids. EP3FL is a good thermal and electrical insulator. The color of EP3FL is tan to brown. Its service temperature range is -100°F to +300°F. This epoxy system is useful in aerospace, electronic, electrical and specialty OEM applications, particularly when bonding dissimilar substrates that are subjected to thermal cycling and shock.

Product Advantages

  • Single component system; no mixing required
  • Unlimited working life at room temperature
  • Fast curing
  • Can withstand rigorous thermal cycling
  • Good low temperature serviceability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.