EP3HTFL
One component epoxy system for bonding, sealing and coating
Key Features
- No mixing and convenient processing
- Toughened system
- Wide service temperature range of -80°F to +350°F
- Superb thermal and electrical insulator
Typical Properties
Viscosity
100,000-200,000 cps
Cure Schedule
250°F for 20-30 minutes, 300°F for 5-10 minutes
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +350°F
Dielectric Constant
3.7
Volume Resistivity
>10¹⁴ ohm-cm