EP42HT-2
Two component, room temperature curing epoxy compound
Key Features
- Heat, chemical and steam resistance
- Cures at ambient or elevated temperatures
- Can be used for bonding, sealing, coating, casting & potting applications
- Serviceable from -60°F to +450°F
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 30-70 cps
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
>75 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
3.07 at 9.375GHz
Refractive Index
1.63
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Case Study
Microfluidic Valve-Based Pressure Injector
Master Bond EP42HT-2 was used in research for a microfluidic valve-based pressure injector.