Master Bond EP46HT-2AO Black is a two component epoxy system for demanding bonding, sealing and encapsulation applications where thermal conductivity, electrical insulation and high temperature resistance are required. It is 100% reactive and does not contain any solvents or diluents. EP46HT-2AO Black is formulated to cure rapidly and requires a cure temperature of 250°F or more. An optimal curing schedule is 3-4 hours at 250-300°F followed by a post cure of 2-3 hours at 350-400°F. The glass transition temperature is quite high, between 140-150°C, and the service temperature range is -100°F to +500°F. Once cured, EP46HT-2AO Black features exceptional physical and mechanical properties, along with exquisite dimensional stability. It bonds well to a wide variety of substrates including metals, glass, ceramics, composites, various rubbers and many plastics. It is a highly functional electrical insulator. It has very good chemical resistance to water, fuels, oils, acids and bases. Most importantly, it passes NASA low outgassing testing. The color of Part A is black and Part B is gray. This high powered combination of product properties allows this system to be used in challenging applications in aerospace, electronics, optoelectronics and in vacuum environments.
Product Advantages
- Extremely forgiving mix ratio
- Very long open time at room temperature
- Top notch heat resistance
- Thermally conductive, electrically insulative
- High quality dimensional stability
- Meets NASA low outgassing requirements
- Passes fungus resistance MIL-STD-810G