EP62-1AO
Two component epoxy resin system featuring excellent temperature and chemical resistance
Key Features
- Long open time at room temperature
- Cures rapidly at moderate temperatures
- Thermally conductive, electrically insulating
- NASA low outgassing
Typical Properties
Viscosity
paste
Cure Schedule
4-6 hours at 140-160°F, 20-40 minutes at 175-200°F or 10-20 minutes at 250-300°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.8
Tensile Lap Shear Strength
800-1,000 psi