EP79FL
Two component, room temperature curing epoxy for bonding, sealing and coating
Key Features
- Very low volume resistivity
- Outstanding flexibility
- Cost effective
- Silver coated nickel filled system
- Withstands rigorous thermal cycling
- Superior T-peel strength
Typical Properties
Viscosity
flowable
Cure Schedule
overnight at 75°F followed by a heat cure of 2-3 hours at 200°F
Hardness
>50 Shore D
Service Temperature Range
4K to +275°F
Thermal Conductivity
12-15 BTU•in/(ft²•hr•°F) [1.73-2.16 W/(m•K)]
Volume Resistivity
<0.005 ohm-cm