MasterSil 920-LO
One part, low outgassing, low stress silicone system for coating, sealing & encapsulating
Key Features
- Meets NASA ASTM E595
- Moderate viscosity with good flow properties
- Neutral type cure
- Superb optical clarity
Typical Properties
Viscosity
5,000-10,000 cps
Cure Schedule
Recommended cure time, 75°F: 7 days
Hardness
25-35 Shore A
Service Temperature Range
-175°F to +500°F
Dielectric Constant
2.5
Refractive Index
1.43
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Packaging
Vídeo
The Latest High Performance Silicone Adhesive System MasterSil 920-LO
NASA low outgassing compliant, MasterSil 920-LO is an ideal material for the encapsulation of sensitive electronic and optical components, especially when low stress is a critical requirement.
This neutral curing, RTV silicone has very good flow pr …