MB297
High viscosity ethyl cyanoacrylate with excellent performance profile
Key Features
- One component, non-mix system
- Top level adhesion to a wide variety of substrates
- Fast setting with rapid fixture time
- Industrial grade
Typical Properties
Viscosity
2,200-2,400 cps
Cure Schedule
Set up time, 75°F 20-50 seconds (substrate dependent)
Hardness
70 Shore D
Service Temperature Range
-60°F to +250°F
Tensile Lap Shear Strength
1,150 psi
Volume Resistivity
>10¹⁵ ohm-cm