Steelmaster 43HT
Two component, room temperature curing, stainless steel filled epoxy
Key Features
- For repairing, rebuilding and resealing
- Cures at ambient temperature
- High bond and compressive strength
- Convenient packaging
Typical Properties
Viscosity
Part A: 50,000 - 100,000 cps, Part B: paste
Cure Schedule
cure readily in about 24-48 hours at 75°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
2,400-2,600 psi
Tensile Modulus
500,000-550,000 psi