Supreme 11HT
Toughened, two component epoxy for bonding, sealing and coating
Key Features
- Excellent toughness
- Convenient handling
- High bond strength in shear and peel modes
- Thermal stabilty up to +400°F
- Withstands thermal cycling
- Superb adhesion to many substrates
Typical Properties
Viscosity
Part A: 90,000-120,000 cps, Part B: 60,000-110,000 cps
Cure Schedule
overnight at 75°F, followed by 1 hour at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-112°F to +400°F
Coefficient of Thermal Expansion
45-50 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
Imagen