Supreme 3ANLV-1
One component, flowable thermally conductive, electrically insulating epoxy for bonding and sealing
Key Features
- Superior heat transfer properties
- Convenient processing
- Fast curing at moderately elevated temperatures
- Withstands thermal cycling
Typical Properties
Viscosity
125,000-175,000 cps
Cure Schedule
Cures readily at 250°F in 20-30 minutes and at 300°F in 5-10 minutes.
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +300°F
Coefficient of Thermal Expansion
35-40 x 10⁻⁶ in/in/°C
Dielectric Constant
4.2
Dielectric Strength
450 volts/mil
T-peel Strength
5-10 pli
Tensile Lap Shear Strength
1,000-1,200 psi
Tensile Modulus
325,000-425,000 psi
Thermal Conductivity
23-24 BTU•in/(ft²•hr•°F) [3.32-3.46 W/(m•K)]
Volume Resistivity
>10¹⁵ ohm-cm