UV15-7NV-2

One part UV system for high performance bonding, sealing, coating and encapsulation
Key Features
  • Low viscosity
  • Strong adhesive
  • Excellent physical properties, enhanced durability and toughness
  • Low shrinkage upon cure
Typical Properties
Viscosity
500-2,500 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
70-80 Shore D
Service Temperature Range
-80°F to +300°F
Coefficient of Thermal Expansion
55-60 X 10⁻⁶ in/in/°C
Refractive Index
1.54
Image
UV Adhesive System UV15-7NV-2
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15-7NV-2 is a one component, UV curable polymer system for high performance bonding, sealing, coating and encapsulation. It has good physical strength properties, low shrinkage upon curing and is non-yellowing. This system bonds well to a wide variety of substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of polyester films. It is 100% reactive and does not contain any solvents or diluents. UV15-7NV-2 offers very good chemical resistance to water, fuels and many solvents. The UV cured polymeric material can be employed over the wide service temperature range of -80°F to +300°F. UV15-7NV-2 exhibits an excellent combination of properties including outstanding toughness, electrical insulation and withstands thermal cycling.

Master Bond UV15-7NV-2 system is not oxygen inhibited and generally cures in 15-45 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections up to 1/8 inch. However when bonding, sections of a few thousandths of an inch are more than adequate. This system is widely used in optical, fiber-optic, electronic, laser, microelectronic and semiconductor applications.

 

Product Advantages

  • Fast cure upon exposure to a UV light source
  • No oxygen inhibition
  • Superb electrical insulator
  • Exceptional bond strength with good toughness
  • Good dimensional stability
  • Outstanding clarity and light transmission
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.