UV15DC80-1Med
One component, moderate viscosity, UV and heat curable epoxy compound that meets ISO 10993-5 for medical device applications
Key Features
- Allows for curing in “shadowed out” areas
- Cures at temperatures as low as 80°C
- Convenient no mix system
- Excellent physical strength properties
Typical Properties
Viscosity
20,000-40,000 cps
Cure Schedule
Cure at 80°C for 40-60 minutes; Additional post curing at 80°C for 2-4 hours or 125°C for 30-60 minutes
Hardness
>70 Shore D
Service Temperature Range
-80°F to +350°F
Dielectric Constant
3.49
Refractive Index
1.52