News Releases

Stay informed about Master Bond's latest product developments, company events, and other exciting announcements.
 

Release Date:
Product: EP21FRNS-2

Featuring a non-halogen filler, Master Bond EP21FRNS-2 passes UL 94V-0 testing for flame retardancy in potting, encapsulation and casting applications. It produces very low smoke levels and is well suited for the computer, aerospace and related industries.

This two part epoxy features a convenient one to one mix ratio…

Release Date:
Product: FLM36

In an effort to mitigate the more complicated preparation associated with B-staged epoxies, Master Bond developed FLM36 for bonding and sealing applications in the aerospace, electronic, opto-electronic and specialty OEM industries. This B-staged film eliminates mixing and measuring and is easy to handle.

FLM36 can…

Release Date:
Product: UV25

Suitable for high production applications, Master Bond UV25 offers fast fixture times, rapid curing and high temperature resistance. This multifunctional one component UV curable system was developed for bonding, sealing, coating and encapsulation applications. It is widely used in aerospace, fiber-optic, optical, electronic and…

Release Date:
Product: Super Gel 9

Featuring softness and resilience, Master Bond Super Gel 9 is a urethane modified epoxy gel that can be employed in a variety of applications. Some of the most common include the encapsulation of sensitive electronic parts and sealing optical components. This multifunctional system is also widely used in the aerospace, electronic…

Release Date:
Product: EP62-1

With the ability to withstand acids, bases and many solvents, Master Bond EP62-1 is primarily used as an adhesive, sealant or coating where the epoxy will be exposed to very harsh conditions. This two part epoxy features thermal stability with a glass transition temperature in the range of 120-130°C.

EP62-1 has a long…