One Part High Strength Epoxy With High Thermal Conductivity Meets NASA Low Outgassing Specifications
Resistance to impact, thermal shock, vibration and stress fatigue cracking is of vital importance in the aerospace, optical, medical and oil/chemical processing industries. Master Bond Polymer Adhesive Supreme 10AOHT-LO is a single component, no mix, thermally conductive compound featuring superior electrical insulation and toughness.
It meets NASA low outgassing specifications and has superior durability and dimensional stability. It is formulated to cure at elevated temperatures between 250°F and 300°F for 1 hour, and produces exceptional bonds for service over the wide temperature range of 4K to 400° F. These tough bonds are remarkably resistant to severe thermal cycling and many chemicals, including water, oil and various fuels.
The hardened adhesive is a superb thermal conductor with a thermal conductivity of 9-10 BTU /in/ft²/hour/°F. Its Shore D hardness exceeds 75 and its compressive strength is greater than 15,000 psi. It is available for purchase in half pints, pints, quarts, gallons and 5 gallon containers.
For Editorial Use
Click below to download this release in the format of your choice.
| Élément joint | Taille |
|---|---|
| su10aoht-lo_nr.doc (22 KB) | 22 KB |
| Élément joint | Taille |
|---|---|
| su10aoht-lo_nr.html (3.29 KB) | 3.29 KB |
| Élément joint | Taille |
|---|---|
| su10aoht-lo_nr.txt (2.55 KB) | 2.55 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.