Supreme 10HT One Part Epoxy
Supreme 10HT
One component, toughened epoxy system
Glass Transition Temperature (Tg)
130-135°C
Tensile Lap Shear Strength
3,600-3,800 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 60-75 minutes at 250°F; 35-40 minutes at 300°F 70-80 Shore D 4K to +400°F /fr/tds/supreme-10ht
Supreme 10HTCL Single Component Epoxy
Supreme 10HTCL
One component, heat resistant toughened epoxy system passes NASA low outgassing
Tensile Lap Shear Strength
2,800-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
140,000-200,000 cps 60-75 minutes at 250°F 70-80 Shore D 4K to +400°F /fr/tds/supreme-10htcl
Supreme 10HTF-1 One Part Epoxy Compound
Supreme 10HTF-1
One component, fast curing, toughened epoxy adhesive/sealant
Tensile Lap Shear Strength
>3,200 psi
Tensile Modulus
350,000-400,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 5-10 minutes at 300°F or 15-20 minutes at 250°F; post cure at 250-300°F for 1-2 hours >70 Shore D 4K to +400°F /tds/supreme-10htf-1
Supreme 10HTFL One Component Epoxy
Supreme 10HTFL
One component, flexibilized epoxy system
Dielectric Constant
4.5
T-peel Strength
40-50 pli
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
350,000-700,000 cps 20-30 minutes at 300°F or 45-60 minutes at 250°F 45-65 Shore D 4K to +350°F /fr/tds/supreme-10htfl
Supreme 10HTLV One Part Epoxy System
Supreme 10HTLV
One component, toughened epoxy system
Tensile Lap Shear Strength
3,600-3,800 psi
Volume Resistivity
>10¹² ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
200,000-400,000 cps 60-75 minutes at 250°F; 35-40 minutes at 300°F 70-80 Shore D 4K to +400°F /fr/tds/supreme-10htlv
Supreme 10HTN One Part Epoxy
Supreme 10HTN-NV
One component, heat curing, nickel conductive epoxy system
Tensile Lap Shear Strength
1,200-1,400 psi
Volume Resistivity
5-10 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste minimum 250°F for 60-90 minutes 85-95 Shore D 4K to 400°F /fr/tds/supreme-10htn-nv
Supreme 10HTND-3 One Part Epoxy
Supreme 10HTND-3
One component, toughened epoxy system
Tensile Strength
8,000-9,000 psi
Tensile Modulus
450,000-500,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 60-75 minutes at 250°F 75-85 Shore D 4K to +400°F /fr/tds/supreme-10htnd-3
Supreme 10HTS One Part Epoxy
Supreme 10HTS
One component, heat curing, toughened epoxy system
Tensile Lap Shear Strength
>1,200 psi
Volume Resistivity
<0.006 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 250°F for 60-75 minutes, 300°F for 40-45 minutes >75 Shore D 4K to +400°F /fr/tds/supreme-10hts
Supreme 12AOHT-LO Epoxy System
Supreme 12AOHT-LO
One part, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing; meets NASA low outgassing specifications
Glass Transition Temperature (Tg)
135-140°C
Tensile Lap Shear Strength
3,400-3,600 psi
  • 1,000 Hours at 85°C/85% RH
  • MIL-STD-883J for Thermal Stability
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 125°C (257°F) in 60-70 minutes and 150°C (302°F) in 40-50 minutes 80-90 Shore D 4K to +500°F /fr/tds/supreme-12aoht-lo
One Part Epoxy System
Supreme 17HT
One component toughened epoxy system for bonding and sealing
Glass Transition Temperature (Tg)
208-210°C
Tensile Lap Shear Strength
1,900-2,100 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
100,000-150,000 cps 300°F for 4-6 hours, plus 8-12 hours at 350°F. 80-90 Shore D -100°F to +550°F /fr/tds/supreme-17ht