EP93FRHT Two Component Epoxy
EP93FRHT
Two component epoxy system meets the Airbus standards noted below from ABD0031, Issue F, June 8, 2005 for flame retardancy
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm
  • Airbus Standards for Flame Retardancy
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Casting
  • Gap Filling
6,000-9,000 cps overnight at 75°F followed by 3-5 hours at 150-200°F 80-90 Shore D -80°F to +400°F /fr/tds/ep93frht
Super Gel 9 Two Part Urethane Modified Epoxy
Super Gel 9
Two component urethane modified epoxy gel-like system
Dielectric Strength
>420 volts/mil
Refractive Index
1.5253
  • RoHS Compliant
  • Bonding
  • Sealing
  • Casting
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
3,000-9,000 cps cures at 75°F, 4-7 days <5 Shore A -100°F to +200°F /fr/tds/super-gel-9
Supreme 112: two part epoxy for bonding, sealing, potting and impregnation
Supreme 112
Two part epoxy for bonding, sealing, potting and impregnation requires elevated temperature curing
Glass Transition Temperature (Tg)
190-195°C
Volume Resistivity
>10¹⁴ ohm-cm at 25°C, >10¹² ohm-cm at 150°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Impregnation
  • Coating
  • Encapsulation
  • Gap Filling
50-200 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F 75-90 Shore D -80°F to +550°F /fr/tds/supreme-112
Supreme 11AOHT Two Part Epoxy
Supreme 11AOHT
Two component thermally conductive, electrically insulative epoxy compound for bonding, coating and sealing
Dielectric Constant
4.6
Tensile Lap Shear Strength
3,200-3,400 psi
  • MIL-STD-883J for Thermal Stability
  • RoHS Compliant
  • Bonding
  • Coating
  • Sealing
  • Gap Filling
Part A: 200,000-300,000 cps, Part B: paste 8-12 hours at 75°F, plus 1-2 hours at 150-200°F 80-85 Shore D -112°F to +400°F /fr/tds/supreme-11aoht
Supreme 11AOHT-LO Two Part Epoxy System
Supreme 11AOHT-LO
Toughened, high strength, two component epoxy for bonding and sealing
Coefficient of Thermal Expansion
35-40 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
Part A: 200,000-300,000 cps, Part B: paste overnight at 75°F followed by a few hours at 150-200°F 80-90 Shore D -112°F to +400°F /fr/tds/supreme-11aoht-lo
Supreme 11AOHTLP Two Part Epoxy
Supreme 11AOHTLP
Two component, thermally conductive, electrically insulative epoxy for bonding, sealing and coating
Dielectric Constant
4.6
Tensile Modulus
400,000-450,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 3-4 hours at 150-200°F 85-90 Shore D -112°F to +400°F /fr/tds/supreme-11aohtlp
Master Bond Supreme 11AOHTMed Epoxy System
Supreme 11AOHTMed
Toughened, high strength, two component epoxy for bonding and sealing
Dielectric Constant
4.6
T-peel Strength
15-20 pli
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 200,000-300,000 cps, Part B: paste 75°F: 24-36 hours; 200°F: 1-2 hours 80-90 Shore D -112°F to +400°F /fr/tds/supreme-11aohtmed
Supreme 11HT Two Part Epoxy
Supreme 11HT
Toughened, two component epoxy for bonding, sealing and coating
Coefficient of Thermal Expansion
45-50 X 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
3,200-3,400 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 90,000-120,000 cps, Part B: 60,000-110,000 cps overnight at 75°F, followed by 1 hour at 150-200°F 75-85 Shore D -112°F to +400°F /fr/tds/supreme-11ht
Two Part Epoxy Supreme 121AO
Supreme 121AO
Two part toughened epoxy for bonding, sealing and encapsulation features good thermal conductivity
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F)
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
10,000-25,000 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. 85-95 Shore D -80°F to +550°F /fr/tds/supreme-121ao
Two Part Epoxy Supreme 121AOMed
Supreme 121AOMed
Two part toughened epoxy for bonding, sealing and potting featuring good thermal conductivity and high temperature resistance; requires oven curing
Glass Transition Temperature (Tg)
200-210°C
Thermal Conductivity
4-5 BTU•in/(ft²•hr•°F) [0.58-0.72 W/(m•K)]
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
10,000-25,000 cps 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Additional post curing at 350°F for 2-4 hours will further enhance product properties. 85-95 Shore D -80°F to +550°F /fr/tds/supreme-121aomed

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).