EP41S-5 Two Part Epoxy System
EP41S-5
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
140-145°C
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Casting
  • Encapsulation
  • Gap Filling
25,000-30,000 cps overnight at 75°F followed by 3-4 hours at 150-200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5
Low viscosity, chemically resistant epoxy system EP41S-5LV
EP41S-5LV
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Glass Transition Temperature (Tg)
120-125°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
2,000-5,000 cps 75°F: 3-5 days; 150-200°F: 2-3 hours 85-95 Shore D -80°F to +350°F /tds/ep41s-5lv
Two Part Epoxy EP41S-5Med
EP41S-5Med
Two component epoxy system featuring excellent resistance to sterilants, solvents and autoclaving
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
140-145°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
25,000-30,000 cps 75°F: 3-5 days; 150-200°F: 2-3 hours; Optimal cure schedule: overnight at 75°F, plus 3-4 hours at 200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5med
EP41S-5ND Black Two Part Epoxy
EP41S-5ND Black
Two component epoxy system featuring excellent chemical resistance especially to solvents, acids, bases, alcohols and fuels
Glass Transition Temperature (Tg)
140-145°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Encapsulation
Part A: paste, Part B: paste overnight at 75°F followed by 3-4 hours at 150-200°F 85-95 Shore D -80°F to +450°F /tds/ep41s-5nd-black
EP41S-6
Two component epoxy system that meets UL 1203 for Explosion-Proof and Dust-Ignition-Proof Electrical Equipment for Use in Hazardous (Classified) Locations
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
145-150°C
  • RoHS Compliant
  • UL 1203 for Explosion-Proof & Dust-Ignition-Proof
  • Bonding
  • Casting
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
  • Sealing
30,000-60,000 cps 24 hours at room temperature followed by 10 hours at 125°C 85-95 Shore D -80°F to +500°F /tds/ep41s-6
EP41S-LO Two Part Epoxy Compound
EP41S-LO
Versatile two part epoxy system for bonding, sealing, coating and potting that meets NASA low outgassing specifications
Tensile Modulus
300,000-350,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
Part A: 10,000-15,000 cps, Part B: 3,000-5,000 cps cures in 24 hours at 75°F, in 60-90 minutes at 200°F >75 Shore D -60°F to +250°F /fr/tds/ep41s-lo
EP41SMed Two Component Epoxy System
EP41SMed
Two part epoxy system for bonding, sealing, coating and potting that meets USP Class VI and ISO 10993-5 for medical applications
Dielectric Constant
3.6
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
Part A: 10,000-15,000 cps, Part B: 3,000 - 5,000 cps 24 hours at 75°F, 60-90 minutes at 200°F, optimum cure schedule overnight at 75°F followed by 1-2 hours at 150-200°F >75 Shore D -60°F to +250°F /fr/tds/ep41smed
EP42-2LV Two Part Epoxy
EP42-2LV
Two component, room temperature curing epoxy compound featuring low viscosity and superior chemical resistance
Refractive Index
1.61
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
Part A: 10,000-15,000 cps, Part B: 30 - 70 cps cures at ambient or elevated temperatures, with the optimum being overnight at 75°F followed by 2-4 hours at 150-200°F 75-85 Shore D -60°F to +350°F /fr/tds/ep42-2lv
 EP42-2LV Black Two Component Epoxy
EP42-2LV Black
Two component, room temperature curing epoxy compound featuring low viscosity and superior chemical resistance
Dielectric Constant
4.0
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Potting
  • Gap Filling
  • Encapsulation
1,000-2,000 cps 75°F: 48-72 hours, 200°F: 2-3 hours, Optimum cure schedule: overnight at 75°F plus 2-4 hours at 150-200°F 80-90 Shore D -60°F to +350°F /fr/tds/ep42-2lv-black
EP42HT-2 Two Part Epoxy
EP42HT-2
Two component, room temperature curing epoxy compound
Dielectric Constant
3.07 at 9.375GHz
Refractive Index
1.63
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
Part A: 55,000-110,000 cps, Part B: 30-70 cps 75°F: 48-72 hours; 200°F: 2-3 hours >75 Shore D -60°F to +450°F /fr/tds/ep42ht-2

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).