MB297Med-1 One Part Ethyl Cyanoacrylate Adhesive
MB297Med-1
Moderate viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,100 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
1,000-1,100 cps Set up time, 75°F 15-45 seconds (substrate dependent) 70 Shore D -60°F to +250°F /fr/tds/mb297med-1
MB297Med-2 One Part Ethyl Cyanoacrylate Compound
MB297Med-2
Lower viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,050 psi
Volume Resistivity
>10¹⁵ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
100-110 cps Set up time, 75°F 10-40 seconds (substrate dependent) 70 Shore D -60°F to +250°F /fr/tds/mb297med-2
MB297Med-3 Single Component Ethyl cyanoacrylate
MB297Med-3
Very low viscosity ethyl cyanoacrylate for medical device bonding applications
Tensile Lap Shear Strength
1,230 psi (ABS-ABS)
Volume Resistivity
>10¹⁵ ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
10-20 cps Set up time, 75°F 5 to 35-40 seconds (substrate dependent) 70 Shore D -60°F to +250°F /fr/tds/mb297med-3
MB600G One Part Sodium Silicate Coating
MB600G
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
1.53
Surface Resistivity
1-10 ohm
  • RoHS Compliant
  • Coating
Paste 75°F 24-48 hours, 175°F (do not exceed 175°F) 1-2 hours 0°F to +700°F /fr/tds/mb600g
MB600S One Part Sodium Silicate System
MB600S
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
4.4
Surface Resistivity
<1 milliohm
  • RoHS Compliant
  • Coating
Paste 75°F: 24-48 hours; 175°F (do not exceed 175°F): 1-2 hours 0°F to +700°F /fr/tds/mb600s
MB600SCN One Part Sodium Silicate Coating
MB600SCN
One component, electrically conductive sodium silicate, aqueous based coating system
Specific Gravity
3.0
Surface Resistivity
<10 milliohm
  • RoHS Compliant
  • Coating
paste 75°F: 24-48 hours; 175°F (do not exceed 175°F): 1-2 hours 0°F to +700°F /tds/mb600scn
Super Gel 9 Two Part Urethane Modified Epoxy
Super Gel 9
Two component urethane modified epoxy gel-like system
Dielectric Strength
>420 volts/mil
Refractive Index
1.5253
  • RoHS Compliant
  • Bonding
  • Sealing
  • Casting
  • Encapsulation
  • Potting
  • Coating
  • Gap Filling
3,000-9,000 cps cures at 75°F, 4-7 days <5 Shore A -100°F to +200°F /fr/tds/super-gel-9
Supreme 10AOHT One Part Epoxy System
Supreme 10AOHT
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing
Tensile Lap Shear Strength
3,400-3,600 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-85 Shore D 4K to +400°F /fr/tds/supreme-10aoht
Supreme 10AOHT-LO One Part Epoxy System
Supreme 10AOHT-LO
One component, thermally conductive, electrically insulating, high performance epoxy for bonding and sealing meets NASA low outgassing specifications
Dielectric Constant
4.3
Tensile Lap Shear Strength
3,400-3,600 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
paste 250°F for 60-70 minutes, 300°F for 40-50 minutes 80-90 Shore D 4K to +400°F /fr/tds/supreme-10aoht-lo
Supreme 10HT One Part Epoxy
Supreme 10HT
One component, toughened epoxy system
Glass Transition Temperature (Tg)
130-135°C
Tensile Lap Shear Strength
3,600-3,800 psi
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
>500,000 cps 60-75 minutes at 250°F; 35-40 minutes at 300°F 70-80 Shore D 4K to +400°F /fr/tds/supreme-10ht