Lab Report

Testing Adhesives for Resistance to Nitric Acid

Many Master Bond epoxy systems are formulated with superior acid resistance. We continually test our materials by exposing them to specific chemicals over a long period of time. A common way of testing the chemical compatibility of an epoxy is by immersing a sample in a chemical and measuring its change in weight over time. A significant loss or gain in weight would indicate a decreased ability of a material to stand up to chemical exposure. These tests allow us to more accurately recommend the right product based on specific application requirements.

IIn this experiment, we focused on testing our epoxies for their resistance to nitric acid. The compounds Master Bond used for testing are a variety of two-component and one-component epoxies with good overall chemical resistance. For the first round of testing, which involved exposure to 10% nitric acid, the products tested were EP125, EP62-1HT, EP21ARHT, EP62-1BF, EP17HT, and EP41S-5. For the second round of testing, which involved exposure to 20% nitric acid, the same products were tested. For both tests, these products were compared against the resistance of a generic or standard non-chemically resistant epoxy. A few thin castings were made for each product and cured in accordance with their specifications. Once the cured samples were created and initial weight was recorded, the castings were immersed in either 10% or 20% nitric acid. Then, we continued recording frequent weight measurements. Below you will see the results of soaking for more than one year in each concentration at room temperature ~ 75°F. The castings were weighed periodically, and the graphs shown below demonstrate the percentage of weight change over time.

Testing Adhesives for resistance to Nitric Acid 10%

Testing Adhesives for resistance to Nitric Acid 10%

Testing Adhesives for resistance to Nitric Acid 20%

Testing Adhesives for resistance to Nitric Acid 20%

For comparison, note that for each concentration, a casting of a standard epoxy was also tested under these same conditions which served as a reference. As can be seen in the graphs, the standard epoxy was markedly less resistant to nitric acid than the other epoxies tested. It demonstrated a significantly greater change in weight over time, and at both 10% and 20% concentration levels, the casting ultimately dissolved in nitric acid after approximately seven months.

Acids can etch the surface of an epoxy (resulting in loss of weight), or they can cause swelling of the sample (resulting in weight gain). In general, a weight change of less than 4-5% (gain or loss) can be considered excellent, especially since these tests may be more rigorous compared to actual service conditions. It is also worth noting that in the context of a bonded joint or a potted assembly the exposure to nitric acid might not be as severe or direct as in the above test conditions.

Please note, when choosing an epoxy for an application where the resistance to nitric acid is critical, many other factors must be considered in addition to the chemical resistance. Depending on the concentration level of nitric acid, each of the epoxies in the charts above offers a distinct set of performance properties. For example, at both 10% and 20% concentrations, if electrical insulation and high temperature resistance are needed, EP125 may be a good option. If moderate viscosity and a moderate heat cure is needed EP62-1HT can be considered. If a one-part system is needed at either concentration, EP17HT is an excellent candidate. These products all need to be processed or cured differently but the key in all cases is the addition of heat for enhancing/optimizing chemical resistance especially to nitric acid.

Disclaimer: The findings in this article are not meant to be used for specification purposes.

Nitric Acid Resistant Adhesives

Image
Epoxy System EP125
Structural epoxy adhesive resists temperatures up to 500°F. Exceptional durability and flexural strength. High adhesion to metallic and non-metallic substrates. Heat curable system. Tg +190-200°C. Special two part epoxy with very long working life. Excellent compressive strength. Service operating temperature range from -80°F to +600°F.
תמונה
EP62-1HT Two Part Epoxy
Superior resistance to harsh chemicals, particularly to acids. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-160°C. Shore D hardness 80-90.
תמונה
EP21ARHT Two Part Epoxy
Serviceable from +400°F. Exceptional acid resistance. Cures at room temperature. Good flow properties. 100% reactive. Low shrinkage upon cure. Withstands 1,000 hours 85°C/85% RH. Reliable electrical insulator. Adheres well to metals, glass, ceramics, rubbers and plastics. Shore D hardness 80-90.
תמונה
EP62-1BF Two Component Epoxy
Cures rapidly at moderate elevated temperatures. Superior resistance to harsh chemicals. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +500°F. Tg 170-175°C. Shore D hardness 80-90.
Image
One Part Epoxy System EP17HT
Serviceable up to 600°F. Exceptional Tg of 220-225°C. No mix formulation. Low exotherm upon curing. Exemplary chemical resistance. Can be used in encapsulations and castings beyond 1/2 inch thickness.
תמונה
EP41S-5 Two Part Epoxy System
Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.