Thermally Conductive, Electrically Insulative Two Part Silicone Meets NASA Low Outgassing Specifications
Master Bond MasterSil 972TC-LO passes the rigorous requirements for low outgassing per ASTM E595 specifications. It is particularly well suited for use in vacuum environments as well as applications in the aerospace, electronic, opto-electronic and specialty OEM industries. This two part silicone system offers convenient handling for bonding, sealing, coating and potting.
MasterSil 972TC-LO is an electrically insulator that has a thermal conductivity of 7-9 BTU•in/ft²•hr•°F [1.01-1.30 W/(m•K)]. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers as well as many types of and plastics. Highly flexible, MasterSil 972TC-LO has an elongation of 40-80%, withstands aggressive thermal cycling and resists mechanical shock. This heat dissipative silicone system has a wide service temperature range is -120°F to +400°F.
This addition cured system does not require air for cross-linking. It features low shrinkage upon curing even in thick or wide cross sections. MasterSil 972TC-LO has a moderate viscosity of 30,000-40,000 cps with good flow properties and has a one to one mix ratio by weight. It has a long working life of 6-10 hours at room temperature. This compound is 100% solids and has a white color. Mastersil 972TC-LO is available in 50 gram syringe kits with additional sizes upon request.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| MasterSil 972TC-LO.doc (28.69 KB) | 28.69 KB |
| צְרוּפָה | גודל |
|---|---|
| MasterSil 972TC-LO.html (28.68 KB) | 28.68 KB |
| צְרוּפָה | גודל |
|---|---|
| MasterSil 972TC-LO.txt (341 bytes) | 341 bytes |
News Release Images
Click an image to download a high resolution version in JPEG format.