Toughened, One Component Epoxy Features High Bond Strength and Cryogenic Serviceability
Combining simple handling properties with high strength, Master Bond Supreme 10HTF-1 is a single part adhesive/sealant for a variety of applications in the aerospace, electronic, optical, specialty OEM and related industries. At room temperature, this smooth paste system has an “unlimited” working life and cures rapidly at elevated temperatures. For example, typical cure schedules for Supreme 10HTF-1 are 5-10 minutes at 300°F or 15-20 minutes at 250°F.
Supreme 10HTF-1 delivers impressive physical strength values for tensile lap shear, tensile and T-peel of >3,200 psi, 6,500-7,500 psi and 20-25 pli, respectively. This system bonds well to a wide variety of substrates including metals, composites, glass, ceramics, rubbers and many plastics. It has very low shrinkage upon curing, is dimensionally stable and has a Shore D hardness >70. As a toughened system, Supreme 10 HTF-1 is capable of withstanding rigorous thermal cycling as well as mechanical shock and vibration.
Supreme 10HTF-1 offers cryogenic serviceability over the wide temperature range of 4K to +400°F. The adhesive resists an array of chemicals such as water, fuels, acids, bases and many solvents. Also, it is a reliable electrical insulator. Volume resistivity is 1013 ohm-cm.
This compound is gray, but other colors are available. Supreme 10HTF-1 is available in standard packaging ranging from ½ pint to 5 gallon containers as well as specialty packaging including cartridges and syringes.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| Supreme 10HTF-1_nr.doc (28.68 KB) | 28.68 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme 10HTF-1_nr.html (28.69 KB) | 28.69 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme 10HTF-1_nr.txt (343 bytes) | 343 bytes |
News Release Images
Click an image to download a high resolution version in JPEG format.