EP31

Two component epoxy system featuring exceptional bonding strength properties
Key Features
  • Convenient handling
  • Excellent structural adhesive
  • Combines low viscosity and optical clarity
  • Provides superior electrical insulation values
Typical Properties
Viscosity
Part A: 9,000-15,000 cps, Part B: 10-100 cps
Cure Schedule
cures in about 1-2 days at ambient temperatures, and in about 2-3 hours at 200°F; an overnight cure at 75°F followed by 2-3 hours at 150-200°F is desirable
Hardness
70-80 Shore D
Service Temperature Range
-60°F to +250°F
T-peel Strength
>50 pli
Tensile Modulus
300,000-350,000 psi
תמונה
EP31 Two Component Epoxy System
Product Description

Master Bond EP31 is a two part epoxy system used primarily for bonding, but is also serviceable as a coating, sealing and encapsulation agent. The processing is relatively easy and straightforward with a forgiving mix ratio of 100 to 30 by weight. It cures readily at room temperature or more rapidly at elevated temperatures. At ambient temperatures, it cures in about 1-2 days, and at 200°F, in about 2-3 hours. To optimize properties, an overnight cure at room temperature followed by 2-3 hours at 150-200°F is desirable. Upon cross linking, EP31 has toughness and resiliency allowing it to withstand aggressive thermal cycling. Most prominent is its remarkable tensile lap shear and peel strength (summarized below). It bonds well to a wide variety of substrates, including metals, composites, glass, rubber, ceramics and many plastics. Some other desirable attributes include chemical resistance to water, oils and fuels; very good optical clarity and low shrinkage upon curing. It is a first class electrical insulator, which, when combined with its good flow properties, enables it to be used for smaller potting applications. The service temperature range is -60°F to +250°F. It is also available in a non-drip version called EP31ND. This robust product profile allows EP31 to be considered for use in aerospace, electronic, optical, opto-electronic, specialty OEM and related industries.

Product Advantages

  • User friendly handling and processing
  • Versatile cure schedules
  • Stellar lap shear and peel strength properties
  • Top notch electrical insulation properties
  • Impressive optical clarity
  • Product Citation

    EP31 was cited an article titled “Piezoelectric Microfiber Composite Actuators for Morphing Wings” by Timothy D. Usher, Kenneth R. Ulibarri Jr., and Gilberto S. Camargo at the Department of Physics, California State University at San Bernardino, California. Click here.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.