EP41S-1HT
Two component epoxy adhesive, sealant, coating and encapsulating system
Key Features
- Versatile curing schedules
- Outstanding resistance to solvents
- Impressive physical strength properties
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 60,000-110,000 cps, Part B: 250-400 cps
Cure Schedule
75°F cures in 24-48 hours, 200°F cures in 2-3 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Dielectric Strength
440 volts/mil
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
1,000 Hours at 85°C/85% RH