EP42-2LV
Two component, room temperature curing epoxy compound featuring low viscosity and superior chemical resistance
Key Features
- Easy to use mix ratio
- Cures at ambient or elevated temperatures
- Long working life
- Very good electrical insulator
Typical Properties
Viscosity
Part A: 10,000-15,000 cps, Part B: 30 - 70 cps
Cure Schedule
cures at ambient or elevated temperatures, with the optimum being overnight at 75°F followed by 2-4 hours at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +350°F
Refractive Index
1.61
Volume Resistivity
>10¹⁴ ohm-cm