EP42HT-2AO-1 Black

Two part, room temperature curable epoxy adhesive, sealant, coating and casting system
Key Features
  • Convenient handling, long working life
  • Thermal conductive and electrical insulative
  • Superior thermal stability
  • Passes NASA low outgassing specifications
  • Cryogenically serviceable
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 50,000-120,000 cps, Part B: 200-1,000 cps
Cure Schedule
75°F: 3-5 days; 200°F: 2-3 hours
Hardness
85-90 Shore D
Service Temperature Range
4K to +400°F
Coefficient of Thermal Expansion
18-21 x 10⁻⁶ in/in/°C
Tensile Lap Shear Strength
900-1,100 psi
תמונה
EP42HT-2AO-1 Black Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP42HT-2AO-1 Black is a two component epoxy adhesive, sealant, coating and casting system with a number of noteworthy features. It has a forgiving mix ratio of 100 to 40 by weight along with very good flow properties. It cures readily at ambient temperatures or more rapidly at elevated temperatures. To optimize the properties, the best cure schedule is overnight at room temperature, followed by 2-3 hours at 150-200°F.

EP42HT-2AO-1 Black has good thermal conductivity, while still maintaining excellent electrical insulation values. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers and plastics. Since this system contains filler, an added benefit is enhanced dimensional stability and very low shrinkage upon curing. EP42HT-2AO-1 Black has lower exotherm and is castable to thicknesses up to and exceeding 2-3 inches. It resists chemicals quite well, especially water, oils and fuels. This epoxy is also special in that it is cryogenically serviceable. Its temperature range is 4K to +400°F. Additionally, it meets the NASA low outgassing standard. This highly versatile system can be used in aerospace, electronic, optical, medical, specialty OEM as well as applications where vacuum compatibility is needed.

Product Advantages

  • Relatively easy handling
  • Long working life
  • Good heat conduction
  • Does well in cryogenic applications
  • Can resist higher temperatures
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.