EP46HT-1
Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing
Key Features
- Glass transition temperature of 230-240°C
- Impressive chemical resistance
- Outstanding electrical insulation properties
- Long pot life at room temperature
- Service temperature range of -100°F to +600°F
- High bonding strength
Typical Properties
Viscosity
15,000-35,000 cps
Cure Schedule
250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +600°F
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
230-240°C