EP51
Fast setting, two component epoxy for bonding and sealing
Key Features
- Suitable for bonding and sealing
- Easy handling
- Fast setting, rapid curing
- Cryogenically serviceable
Typical Properties
Viscosity
Part A: 10,000-16,000 cps, Part B: 50,000-75,000 cps
Cure Schedule
75°F: 12-18 hours; 150°F: 30-60 minutes
Hardness
>70 Shore D
Service Temperature Range
4K to +250°F
Dielectric Constant
4.5
Volume Resistivity
>10¹⁴ ohm-cm